  • The CP-8000 Ion Mill Cross Section Polisher gives a perfect finish for SEM sample preparation. Using an argon ion beam, the CP-8000 gently removes material from a sample's surface without deforming or smearing. Easy to use with a touch screen interface.

Get a quote

Product Brochure
  • Please contact us to request a quote or further information
  • Contact Us
Product Overview
  • The COXEM CP-8000 Ion Mill Cross Section Polisher can provide the perfect finish for scanning electron microscopy specimen preparation. Using an argon ion beam, the CP-8000 gently removes material from the surface of a sample, atoms at a time. This gentle process does not deform or smear a sample's surface. Used as a final preparation after mechanical polishing or sectioning, the CP-8000 gives a perfect finish for delicate samples.

    A SEM image of a cross section of material with multiple layers, prepared with mechanical polishing. The surface has been greatly deformed by the mechanical abrasion, obscuring visibility of the individual layers.
    A cross section of multi-layer material, prepared with mechanical polishing
    A SEM image of a cross section of multi-layered composite material, prepared with ion mill polishing. The surface features have been perfectly maintained, with clear visibility of each layer.
    A cross section of multi-layer material, prepared with ion beam polishing

    A CP-8000 is an ideal companion for a COXEM electron microscope, such as the EM-30AX Plus Desktop SEM, to provide perfect sample preparation before sample imaging and analysis.

    Key Features

    • Argon Ion Beam Source
    • Polishes Without Deforming
    • Simple Touch Screen Interface
    • Integrated Chamber Camera
    • Programmable Polishing Recipes
    • Supplied with Alignment Scope

    Intuitive Features & Interface

    With its' user friendly 7" touch screen interface, the CP-8000 is very easy to use. The touch screen GUI is clear and intuitive, and settings can be saved as stored "recipes" to make recurring sample preparation tasks more efficient. An integrated camera allows users to view inside the polisher's chamber and adjust the position of shield plate and specimen.

    Applications

    Ion mill cross selection polishing is commonly used in semiconductor and electronics applications, such as vias, solder joints, bonded layers, and any other situation where softer layers may be deformed by more aggressive mechanical polishing.

    The CP-8000 is also capable of performing delicate cross sectioning of powders, to examine the internal structure in pharmaceutical and materials sciences applications.

Specification
  • Gas Used Ar (argon) Gas
    Milling Speed 150 µm/h (Si at 5kV)
    Accelerating Voltage 2~8 kV
    Beam Diameter Approximately 500 µm
    Working Pressure 2.0 x 10-4 torr
    Beam Alignment Precision beam alignment using fluorescent screen
    Maximum Sample Size 20 x 12 x 7 mm (W x D x H)
    Sample Moving Range Z ± 2 mm
    Y ± 2 mm
    Rotation -35° ~ +35°
    Operation 7 inch touch panel display
    Evacuation System Turbo-molecular pump (66L/s) and Rotary Pump 100L
    Dimensions 590 x 440 x 260 mm (W x D x H)
    Weight Main unit 30kg
    Rotary pump 23kg
    Optional Accessories CCD Camera for viewing the specimen during milling
    Power 110V/ 220V, 50/60Hz, Ground 3V, Capacity 1kVA
    Temperature 20°C ±5°C
    Humidity Less than 70%
    Argon Gas 99.99% of more purity
    Pressure : 3.0 to 4.0 x 10-1 torr
    Ar gas tubing : 1/4-inch SUS piping